Modeling the nanoindentation response of silicate glasses by peridynamic simulations

Yuzhe Cao, Maryam Kazembeyki, Longwen Tang, N. M.Anoop Krishnan, Morten M. Smedskjaer, Christian G. Hoover, Mathieu Bauchy*

*Kontaktforfatter

Publikation: Bidrag til tidsskriftTidsskriftartikelpeer review

1 Citationer (Scopus)
OriginalsprogEngelsk
TidsskriftJournal of the American Ceramic Society
Vol/bind104
Udgave nummer7
Sider (fra-til)3531-3544
Antal sider14
ISSN0002-7820
DOI
StatusUdgivet - jul. 2021