Parametric study of temperature-modulated differential scanning calorimetry for high-temperature oxide glasses with varying fragility

Tobias Kjær Bechgaard, Ozgur Gulbiten, John C. Mauro, Morten Mattrup Smedskjær

Research output: Contribution to journalJournal articleResearchpeer-review

4 Citations (Scopus)
Original languageEnglish
JournalJournal of Non-Crystalline Solids
Volume484
Pages (from-to)84-94
Number of pages11
ISSN0022-3093
DOIs
Publication statusPublished - 15 Mar 2018

Cite this

@article{3d6aefe0ae24418ea41e01364536d902,
title = "Parametric study of temperature-modulated differential scanning calorimetry for high-temperature oxide glasses with varying fragility",
author = "Bechgaard, {Tobias Kj{\ae}r} and Ozgur Gulbiten and Mauro, {John C.} and Smedskj{\ae}r, {Morten Mattrup}",
year = "2018",
month = "3",
day = "15",
doi = "10.1016/j.jnoncrysol.2018.01.022",
language = "English",
volume = "484",
pages = "84--94",
journal = "Journal of Non-Crystalline Solids",
issn = "0022-3093",
publisher = "Elsevier",

}

Parametric study of temperature-modulated differential scanning calorimetry for high-temperature oxide glasses with varying fragility. / Bechgaard, Tobias Kjær; Gulbiten, Ozgur; Mauro, John C.; Smedskjær, Morten Mattrup.

In: Journal of Non-Crystalline Solids, Vol. 484, 15.03.2018, p. 84-94.

Research output: Contribution to journalJournal articleResearchpeer-review

TY - JOUR

T1 - Parametric study of temperature-modulated differential scanning calorimetry for high-temperature oxide glasses with varying fragility

AU - Bechgaard, Tobias Kjær

AU - Gulbiten, Ozgur

AU - Mauro, John C.

AU - Smedskjær, Morten Mattrup

PY - 2018/3/15

Y1 - 2018/3/15

U2 - 10.1016/j.jnoncrysol.2018.01.022

DO - 10.1016/j.jnoncrysol.2018.01.022

M3 - Journal article

VL - 484

SP - 84

EP - 94

JO - Journal of Non-Crystalline Solids

JF - Journal of Non-Crystalline Solids

SN - 0022-3093

ER -