Translated title of the contribution | Tommelfingerregler for 1D-periodiske overflade mikrostrukturer til antirefleksive linser |
---|---|
Original language | English |
Journal | Optics Express |
Volume | 18 |
Issue number | 25 |
Pages (from-to) | 26245-58 |
Number of pages | 14 |
ISSN | 1094-4087 |
DOIs | |
Publication status | Published - 1 Dec 2010 |
Guidelines for 1D-periodic surface microstructures for antireflective lenses
Thomas Søndergaard, Jesper Hølledig Gadegaard, Peter Kjær Kristensen, Thøger Kari Jensen, Thomas Garm Pedersen, Kjeld Pedersen
Research output: Contribution to journal › Journal article › Research › peer-review
10
Citations
(Scopus)