Temperature-Modulated Differential Scanning Calorimetry Analysis of High-Temperature Silicate Glasses: Norbert J. Kreidl Award Lecture

Tobias Kjær Bechgaard, Ozgur Gulbiten, John C. Mauro, Morten Mattrup Smedskjær

Publikation: Konferencebidrag uden forlag/tidsskriftKonferenceabstrakt til konferenceForskningpeer review

58 Downloads (Pure)

Abstract

GOMD-AW-005-2018
OriginalsprogEngelsk
Publikationsdato20 maj 2018
StatusUdgivet - 20 maj 2018
Begivenhed2018 Glass and Optical Materials Division Annual Meeting - Hilton Palacio del Rio, San Antonio, USA
Varighed: 20 maj 201824 maj 2018
http://ceramics.org/gomd2018

Konference

Konference2018 Glass and Optical Materials Division Annual Meeting
LokationHilton Palacio del Rio
Land/OmrådeUSA
BySan Antonio
Periode20/05/201824/05/2018
Internetadresse

Fingeraftryk

Dyk ned i forskningsemnerne om 'Temperature-Modulated Differential Scanning Calorimetry Analysis of High-Temperature Silicate Glasses: Norbert J. Kreidl Award Lecture'. Sammen danner de et unikt fingeraftryk.

Citationsformater